Details pertaining to an orthogonal metal cutting process are given below
Chip thickness ratio 0.4
Undeformed thickness 0.6 mm
Rake angle +10°
Cutting speed 2.5 m/s
Mean thickness of primary shear zone 25 microns
The shear strain rate in s-1 during the process is
Chip thickness ratio 0.4
Undeformed thickness 0.6 mm
Rake angle +10°
Cutting speed 2.5 m/s
Mean thickness of primary shear zone 25 microns
The shear strain rate in s-1 during the process is